Bicycle crankset with 50-34 chainrings and a crank arm, the kind of part a bike brand asks fatigue evidence for before a production order
Photo: Petar Milošević, CC BY-SA 4.0, via Wikimedia Commons (a complete crankset, shown as an example of a fatigue-critical part, not a machined one)

A new bike brand has a design, a launch date and little history with you. Before it places a production order it asks for proof in three layers: a sample it can hold, a first article report that shows the sample met the drawing, and evidence that the part survives riding loads. The shop owns the first two and supports the third. A shop that knows where its responsibility ends, and where the brand’s lab begins, answers faster and promises less. This guide sets out what each layer contains and how to prepare it for bike part first article and sample approval. It builds on the inspection plan guide and the buyer-side view in first article inspection for bike parts.

Diagram: five pieces of evidence a new bike brand asks for, from sample and first article to material records, finish and the brand's fatigue test

Layer 1: the sample

A sample answers two questions: does it fit, and does it look right. Name the drawing revision on the tag, so nobody approves a part against the wrong file. Record the lot code of the bar, the program revision and the finishing route.

Keep a twin. The brand approves a physical piece, and a later color or fit dispute is settled against it. For anodized parts, the color matching guide explains why a physical standard beats a color name. Wikipedia notes that dyed anodize colors vary with the base alloy, and that integral colors cannot be reproduced consistently when the underlying metallurgy changes. That is a reason to send the sample from the same bar source you will use in production.

Say in writing what the sample is: a fit sample, a function sample or a pre-production piece. A fit sample made by a different route than production (for example hand-finished) proves nothing about production, and the brand should know that.

Layer 2: the first article report

First article inspection is a production validation process. Wikipedia describes it as checking that a new or modified process yields parts meeting the drawing, usually performed by the supplier and reviewed by the purchaser. It typically tests and inspects the first part or a sample from the first batch, using calibrated tools such as CMMs, calipers and go/no-go gauges. Material tests such as hardness and conductivity may be required as well.

Bike brands do not have to use the aerospace form set. AS9102, the North American aerospace standard, defines three forms: part number accountability, product accountability and characteristic accountability. Its structure is still a good model, because Form 3 references a ballooned drawing in which each characteristic is uniquely identified. Use the structure, not the paperwork weight.

Report item What to include Common failure
Drawing Ballooned copy at the quoted revision Report written against an older revision
Measured values Every ballooned characteristic, value against limits Only the “critical” ones are listed
Gauges Instrument ID and calibration date Gauge resolution too coarse for the tolerance
Finish Color against the approved sample, thickness on named faces Bore measured before anodize, reported as final
Material Certificate reference, bar lot, temper Certificate from a different lot
Sign-off Name, date and result for each piece Report with no owner

The anodize row catches shops most often. Wikipedia states the oxide grows into and out of the surface in roughly equal amounts, so a 2 μm coating adds about 1 μm to each surface, and it suggests stating that dimensions apply after finishing. Agree with the brand which condition the drawing means, then report in that condition. The growth calculator gives the arithmetic.

Layer 2b: material records

A brand that sells a safety-critical part wants to know what metal it is. Wikipedia describes the mill test report as a quality assurance document certifying a material’s chemical and physical properties, and says EN 10204 type 3.1 certificates declare compliance with the order and give test results, while type 3.2 adds an inspection representative independent of manufacturing together with the purchaser’s representative or an official inspector. That page speaks about steel, so ask your bar supplier what it issues for aluminum bar, and keep the certificate reference with the lot.

Temper matters as much as alloy. Wikipedia lists 7075-T6 at 510 to 540 MPa ultimate tensile strength and T7 at 505 MPa, with T7 less susceptible to stress corrosion cracking because overaging coarsens the precipitates. Our reading: if a brand’s test sample was machined from T6 and you ship T73, you have changed the material the evidence covers. Say so before the order, not after. The 7075 temper guide covers the trade-off.

Need a quote for this part? Get a quote for your bike parts

Layer 3: fatigue evidence, and who owns it

Stems, cranks and steerer clamps carry a rider, and a bike brand needs evidence that its assembly survives repeated loads. ISO 4210-2:2023 sets safety requirements for city and trekking, young adult, mountain and racing bicycles, and its test methods sit in other parts. ISO 4210-5:2023 specifies the steering test methods for ISO 4210-2. For a stem, that is the part to ask the lab about, and its clause text sits behind the standards bodies’ paywall.

The standard tests the bicycle or the assembly. It is not a certificate for a part, and a shop should not describe a part as “ISO 4210 certified”. The brand arranges the test with a lab, and the guide to what brands need from a test lab shows what that conversation looks like from the lab’s side. We could not open the clause text of ISO 4210-5, so we name no test method, load value or cycle count here. Ask the brand’s lab for them.

What the shop controls is whether the parts tested are representative. Wikipedia lists surface finish among the factors influencing fatigue life and notes that identical samples show considerable scatter. On anodizing, it says the effect on fatigue can be significantly negative depending on alloy and coating thickness. Our practical rules:

  • Machine the test parts on the production program, with the production fixture and tooling.
  • Finish them by the production route, including the same anodize type and thickness class.
  • Record lot, temper, revision and finish on a tag, and keep the same record for production lots.
  • Tell the brand when anything in that list changes, and ask whether the evidence still applies.

If you are considering your own rig, read the buy or outsource guide for fatigue test rigs first. Development tests are useful, but a formal report from a lab is what a brand files.

What not to promise

  • Do not call a part certified, approved or compliant on the strength of a first article report. The report says the parts met the drawing, nothing more.
  • Do not quote a fatigue life from memory or from another customer’s part.
  • Do not claim a quality certificate you do not hold.
  • Do not ship production on a different route than the approved sample without telling the brand.

A one-page approval pack

Document Owner Kept with
Approved sample and twin Shop and brand Shelf, tagged with revision and lot
First article report Shop Lot record
Material certificate reference Shop, from the bar supplier Lot record
Finish record Shop or finisher Lot record
Fatigue test report Brand and its lab Brand’s file, copy to shop if the brand agrees

Talk to us

If your shop mills aluminum bike parts and wants to work with new brands that ask for this evidence, read the for suppliers page and talk to us. We will tell you plainly whether your parts and finishing route fit the requests we see.

Sources

Frequently asked questions

Does a machine shop have to run fatigue tests on bike parts?

Usually not. The brand carries the product-level evidence and sends parts to a test lab. The shop's job is to supply parts that represent production: same alloy, temper, finish and drawing revision, with a lot record. If the shop owns a rig, it can run development tests, but a formal test report normally comes from a lab.

How many samples should a shop send a new bike brand?

We found no standard that sets a sample count for brand approval, so agree it in writing. A common split is a few pieces for fit and look, plus a separate set for test work if the brand asks. Keep a twin of every approved piece with the same lot code, so both sides discuss the same part.

What goes in a first article report for a bike part?

A ballooned drawing, the measured value for every characteristic, the gauge used, the material certificate reference, the finish results and a signature with date. First article inspection is a production validation that checks a new or modified process yields parts to the drawing, and the purchaser reviews the report.

Does one fatigue test report cover every later batch?

Only the parts tested. Fatigue results scatter even between seemingly identical samples, and surface finish, alloy and temper all influence life. If the brand changes the drawing revision, the bar source, the temper or the anodize route, ask whether the earlier report still applies before you ship.

Need a quote for this part?

Send the drawing. We quote the finished parts, place the work with a partner shop that machines bike parts and reply within 24 business hours.

Get a quote for your bike parts

Keep reading

Get a quote